James writes - Here is a small batch of moss agates I just finished. This wasn't a full scale operation but I did manage to get a few good looking rocks out of the batch.
They went for 4 weeks in 60/90, (recharged every 7 days) 1 week in 120/220, 1 week in 500 and 1 week in Tin oxide polish. I have to say though, the Tin oxide doesn't work nearly as good on agates, as Titanium oxide does. I'd give them a 7/10 on the shine scale.